Effect of heat treatment to strengthen the alloy aluminum - lithium.
تأثير المعالجة الحرارية على تقوية سبيكة الألمنيوم - ليثيوم.
 
Document Language : Arabic 
Abstract : We have imposed the ambitious goals of modern designs and technical requirements for the production of heavy new generation of aluminum alloys in construction engineering / Almttalba this is above average power to weight, and effective action, and low density, high hardness, and reasonable price. There is a new series of aluminum alloys has been given the numbers 2090, 2091.8090, is currently producing in commercial quantities and meet the requirements above. These alloys less intensity from 8 to 10% and increase the hardness by about 10% from 07,075 conventional alloy. Linked to the strong relationship between the properties and method of treatment with alloy structures that shape formed during the acute treatment of primary as well as sediment rare complex, and the distribution of these deposits depends on the rate of quenching and the degree of cold work prior to aging. So focused research over the past decade the search for better alloys and methods of production, treatment and access to the properties of balanced properties than conventional alloys. Focused research project on the relationship-treatment thermal mechanical property of tensile strength of the alloy of aluminum known as number 08 090 has been testing strain methodology many to see the effect of Cold-start following the process of homogenization (at 454 ° C) and quenching (up to zero degrees centigrade) and the pre-aging unilateralism at 190 Drjo C, and the effect of stretching the double before Altotaiqand 190 Drjo C, as well as prolongation such as heat treatment bilateral aging, which included the peak of aging initial samples Mazalh at 170 ° C and then followed the phase of aging the second raised the temperature to between 200 and 240 degrees Celsius. Has also been testing samples of a single supplement on aging at a temperature of 190 C to peak force and then placed for ten minutes under high temperature up to between 300 and 500 degrees Celsius. Almutalh samples by 7%, such as single-stage aging treatments at a temperature of 190 ° C showed good values ​​of force with little decrease in Almtalah and a significant decline in the space. I have given the aging of the bilateral rates of medium strength they showed in Almtalah Ankhvaza troublesome, and often decrease in size was satisfactory. Oazit weak qualities of high density sludge (Al Li) Almqsbh committed to, as well as the heterogeneous nucleation (Al Li) and (Al Li Cu) T on the borders of beloved. Resulting short exposure to high temperatures after the peak aging at 190 ° C to a significant improvement in Almtalah and a decrease in enrollment and the increase of a reasonable tensile strength. Developed based on these results and the melting of sediments (Al Cu M) S leading to the homogeneity of sliding. Also recorded the results of extensive mechanical tests and scanning electron microscopy and electronic transmission microscope and some X-ray analysis. Conclude from the research that the careful design of mechanical and thermal treatments, which include coordinating a series of rapid, prolongation developed and aging at 170 ° C lead for the best values ​​for the strength and Almtalah. 
Publishing Year : 1413 AH
1993 AD
 
Sponsor Name : kau 
Sponsorship Year : 1413 AH
1993 AD
 
Added Date : Wednesday, April 30, 2008 

Researchers

Researcher Name (Arabic)Researcher Name (English)Researcher TypeDr GradeEmail
طالب يونس ألبalb, taleb yonisInvestigatorDoctorate 

Files

File NameTypeDescription
 30706.docx docx 

Download This Page

Back To Researches Page